YUNGSOX® PP 1924F Homopolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 1924F Homopolymer

YUNGSOX® 1924F is a homopolymer PP resin designed for high-speed thin-wall injection molding, meltblown filters, non-woven fabrics, hygiene materials, and filtration media. It provides 250 g/10 min melt index, 0.90 g/cm³ density, fast cycling, excellent spinnability, and excellent drawability for high-productivity processing.

Associated Documents

TDS - Data Sheet
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Associated Documents

TDS - Data Sheet
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Typical property data

Physical Properties
  • Melt Index: 250 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 300 kg/cm² / 29 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: <50% (ISO 527 / ASTM D-638)
  • Rockwell Hardness: 110 R scale (ISO 2039 / ASTM D-785)
  • Flexural Modulus: 14,000 kg/cm² / 1,373 MPa (ISO 178 / ASTM D-790)
  • IZOD Impact Strength, Notched, 23°C: 2.3 kg·cm/cm / 23 J/m (ISO 180 / ASTM D-256)
Thermal Properties
  • Heat Deflection Temperature: 118°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 149°C (ISO 306)
Certifications & Compliance
  • FDA Food Contact Compliance: FDA 21 CFR 177.1520 for direct food contact

Use & Applications

  • High speed thin walled injection molding products
  • Meltblown filter
  • Non-woven fabric
  • Hygiene
  • Filtration media
fpc taiwan polypropylene pp resin 25kg package