YUNGSOX® 2020 is a homopolymer polypropylene resin designed for BOPP film applications requiring high-speed processing, excellent transparency, and good surface luster. With a melt index of 3 g/10 min, density of 0.90 g/cm³, melting point of 162°C, and haze below 0.12% at 30 μm, YUNGSOX® 2020 PP resin is suitable for food packaging film, garment packaging, transparent tape, and decorative lamination film.