YUNGSOX® PP 2020S Homopolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 2020S Homopolymer Excellent Transparent

YUNGSOX® PP 2020S is a homopolymer PP resin for BOPP film and premium packaging. It supports high-speed processing, excellent transparency, and good luster for food, garment, tape, and laminate film use.

Associated Documents

TDS - Data Sheet
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Typical property data

Physical Properties
  • Melt Index: 3 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 350 kg/cm² / 34 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 600% (ISO 527 / ASTM D-638)
  • Flexural Modulus: 12,500 kg/cm² / 1,226 MPa (ISO 178 / ASTM D-790)
  • Rockwell Hardness: 105 R scale (ISO 2039 / ASTM D-785)
  • IZOD Impact Strength, Notched at 23°C: 4.5 kg·cm/cm / 44 J/m (ISO 180 / ASTM D-256)
Thermal Properties
  • Melting Point: 160°C (DSC)
  • Heat Deflection Temperature: 113°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 150°C (ISO 306)
Optical Properties
  • Haze, 30 μm Film: < 0.11% (FPC Method)
  • Transparency: Excellent transparency
  • Luster: Good luster
Processing Parameters
  • Melt Index for Processing Reference: 3 g/10 min (ISO 1133 / ASTM D-1238)
  • Mold Shrinkage for Processing Design: 1.3–1.7% (FPC Method)
Certifications & Compliance
  • FDA Food Contact Compliance: U.S. FDA 21 CFR 177.1520 for direct food contact
  • JHOSPA-PL Certification

Use & Applications

  • BOPP film
  • high-quality food packaging
  • garment packaging
  • garnish packaging
  • transparent tape