YUNGSOX® PP 2080 Homopolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 2080 Homopolymer IPP Blown Film Food Packaging

YUNGSOX® PP 2080 is a homopolymer PP resin for IPP film, food packaging, and garment packaging. It delivers smooth film handling and clear film appearance. Characteristics: Good antiblocking, Good slippery, Good transparency.

Associated Documents

TDS - Data Sheet
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH

Typical property data

Physical Properties
  • Melt Index: 10 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
Mechanical Properties
  • Tensile Strength at Yield: 350 kg/cm² / 34 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 500% (ISO 527 / ASTM D-638)
  • Rockwell Hardness: 107 R scale (ISO 2039 / ASTM D-785)
  • Flexural Modulus: 14,000 kg/cm² / 1,373 MPa (ISO 178 / ASTM D-790)
  • IZOD Impact Strength, Notched at 23°C: 3.5 kg·cm/cm / 34 J/m (ISO 180 / ASTM D-256)
Thermal Properties
  • Melting Point: 165°C (DSC)
  • Heat Deflection Temperature: 115°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 155°C (ISO 306)
Optical Properties
  • Haze, 30 μm Film: < 2.2% (FPC Method)
  • Transparency Characteristic: Good transparency
Processing Parameters
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Certifications & Compliance
  • FDA Food Contact Compliance: FDA 21 CFR 177.1520 requirements for direct food contact
  • Food Contact Application: Suitable for general food packaging applications

Use & Applications

  • IPP Film
  • General Food Packaging
  • Garment Packaging
fpc taiwan polypropylene pp resin 25kg package

Send Us a Message