YUNGSOX® PP 3003 Impact Copolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 3003 Impact Copolymer

YUNGSOX® PP 3003 is an impact copolymer PP resin with high impact strength and excellent low-temperature toughness. It offers strong melt strength for PPB pipe, thermoforming sheet, and blow molding.

Associated Documents

TDS - Data Sheet
PL JCII Certification
SDS - PP Impact Copolymer
BPA - PP Impact Copolymer
Haolgen - PP Impact Copolymer
PAHs - PP Impact Copolymer
REACH SVHC - PP Impact Copolymer
RoHS - PP Impact Copolymer
EN71-3 - PP Impact Copolymer
EU10-2011 - PP Impact Copolymer
FDA - PP Impact Copolymer
GB4806.6 - PP Impact Copolymer

Typical property data

Physical Properties
  • Melt Index: 0.35 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 250 kg/cm² / 25 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 500% (ISO 527 / ASTM D-638)
  • Rockwell Hardness: 95 R scale (ISO 2039 / ASTM D-785)
  • Flexural Modulus: 13,000 kg/cm² / 1,275 MPa (ISO 178 / ASTM D-790)
  • IZOD Impact Strength, Notched, 23°C: 90 kg·cm/cm / 882 J/m (ISO 180 / ASTM D-256)
  • IZOD Impact Strength, Notched, -20°C: 16 kg·cm/cm / 157 J/m (ISO 180 / ASTM D-256)
Thermal Properties
  • Heat Deflection Temperature: 110°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 145°C (ISO 306)
Processing Parameters
  • Low Melt Index for Processing Stability: 0.35 g/10 min (ISO 1133 / ASTM D-1238)
  • Mold Shrinkage Control: 1.3–1.7% (FPC Method)
Certifications & Compliance
  • FDA Food Contact Compliance: 21 CFR 177.1520

Use & Applications

  • PPB Pipe
  • sheet application
  • blow molding application
fpc taiwan polypropylene pp resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.