Plastic Granules
YUNGSOX® PP 3004 Impact Copolymer
YUNGSOX® PP 3004 is an impact copolymer PP resin for thermoforming and blow molding. It offers high impact strength, excellent melt strength, good stress whitening resistance, and low-temperature toughness.
Associated Documents
TDS - Data Sheet
SDS - PP Impact Copolymer
BPA - PP Impact Copolymer
Haolgen - PP Impact Copolymer
PAHs - PP Impact Copolymer
REACH SVHC - PP Impact Copolymer
RoHS - PP Impact Copolymer
EN71-3 - PP Impact Copolymer
EU10-2011 - PP Impact Copolymer
FDA - PP Impact Copolymer
GB4806.6 - PP Impact Copolymer
Typical property data
Physical Properties
- Melt Index: 0.5 g/10 min (ISO 1133)
- Density: 0.90 g/cm³ (ISO 1183)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 280 kg/cm² (ISO 527)
- Tensile Elongation at Break: >500% (ISO 527)
- Flexural Modulus: 10,500 kg/cm² (ISO 178)
- Rockwell Hardness: 80 R Scale (ISO 2039)
- IZOD Impact Strength, Notched, 23°C: 75 kg·cm/cm (ISO 180)
- IZOD Impact Strength, Notched, -20°C: 10 kg·cm/cm (ISO 180)
Thermal Properties
- Heat Deflection Temperature: 100°C (ISO 75)
- Vicat Softening Temperature: 145°C (ISO 306)
Processing Parameters
- Excellent melt strength
- High impact strength
- Good resistance to stress whitening
- Excellent resistance to low-temperature brittleness
Certifications & Compliance