Plastic Granules
YUNGSOX® PP 3015 Impact Copolymer
YUNGSOX® PP 3015 is an impact copolymer PP resin for pails, luggage bases, sports appliances, and heavy-duty containers. It offers high impact strength, low-temperature toughness, good stiffness, and FDA food-contact compliance.
Associated Documents
TDS - Data Sheet
SDS - PP Impact Copolymer
BPA - PP Impact Copolymer
Haolgen - PP Impact Copolymer
PAHs - PP Impact Copolymer
REACH SVHC - PP Impact Copolymer
RoHS - PP Impact Copolymer
EN71-3 - PP Impact Copolymer
EU10-2011 - PP Impact Copolymer
FDA - PP Impact Copolymer
GB4806.6 - PP Impact Copolymer
Typical property data
Physical Properties
- Melt Index: 2 g/10 min (ISO 1133 / ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 280 kg/cm² / 27 MPa (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 450% (ISO 527 / ASTM D-638)
- Flexural Modulus: 11,500 kg/cm² / 1,128 MPa (ISO 178 / ASTM D-790)
- Rockwell Hardness: 95 R scale (ISO 2039 / ASTM D-785)
- IZOD Impact Strength, Notched at 23°C: 60 kg·cm/cm / 588 J/m (ISO 180 / ASTM D-256)
- IZOD Impact Strength, Notched at -20°C: 13 kg·cm/cm / 127 J/m (ISO 180 / ASTM D-256)
Thermal Properties
- Heat Deflection Temperature: 110°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 145°C (ISO 306)
Flame Characteristics
- UL Flammability Rating: UL 94HB
Processing Parameters
- Melt Index: 2 g/10 min (ISO 1133 / ASTM D-1238)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Certifications & Compliance
- FDA Food Contact Compliance: 21 CFR 177.1520 for direct food contact
Use & Applications
- Pail
- Sports appliance
- Base of luggage