YUNGSOX® PP 3064H Impact Copolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 3064H Impact Copolymer

YUNGSOX® PP 3064H is an impact copolymer PP resin for caps, closures, and appliance parts. It offers high stiffness, strong heat resistance, and reliable impact strength for stable molding performance.

Associated Documents

TDS - Data Sheet
SDS - PP Impact Copolymer
BPA - PP Impact Copolymer
Haolgen - PP Impact Copolymer
PAHs - PP Impact Copolymer
REACH SVHC - PP Impact Copolymer
RoHS - PP Impact Copolymer
EN71-3 - PP Impact Copolymer
EU10-2011 - PP Impact Copolymer
FDA - PP Impact Copolymer
GB4806.6 - PP Impact Copolymer

Typical property data

Physical Properties
  • Melt Index: 6 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 300 kg/cm² / 29 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 200% (ISO 527 / ASTM D-638)
  • Flexural Modulus: 15,500 kg/cm² / 1,520 MPa (ISO 178 / ASTM D-790)
  • Rockwell Hardness: 105 R scale (ISO 2039 / ASTM D-785)
  • IZOD Impact Strength, Notched, 23°C: 15 kg·cm/cm / 147 J/m (ISO 180 / ASTM D-256)
  • IZOD Impact Strength, Notched, -20°C: 4.5 kg·cm/cm / 44 J/m (ISO 180 / ASTM D-256)
Thermal Properties
  • Heat Deflection Temperature: 130°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 155°C (ISO 306)
Processing Parameters
  • Melt Index: 6 g/10 min (ISO 1133 / ASTM D-1238)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Certifications & Compliance
  • FDA Food Contact Compliance: FDA 21 CFR 177.1520 requirements for direct food contact

Use & Applications

  • Automotive parts
  • Electric appliance parts
  • Toys
  • Battery case
  • Furniture
fpc taiwan polypropylene pp resin 25kg package

Send Us a Message