Plastic Granules
YUNGSOX® PP 3080 Impact Copolymer
YUNGSOX® PP 3080 is an impact copolymer PP resin for molded industrial parts. It offers medium impact strength, stable stiffness, and 500% elongation. Suitable for automotive, appliance, battery case, and furniture use.
Associated Documents
TDS - Data Sheet
SDS - PP Impact Copolymer
BPA - PP Impact Copolymer
Haolgen - PP Impact Copolymer
PAHs - PP Impact Copolymer
REACH SVHC - PP Impact Copolymer
RoHS - PP Impact Copolymer
EN71-3 - PP Impact Copolymer
EU10-2011 - PP Impact Copolymer
FDA - PP Impact Copolymer
GB4806.6 - PP Impact Copolymer
Typical property data
Physical Properties
- Melt Index: 8.5 g/10 min (ISO 1133 / ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 280 kg/cm² / 27 MPa (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 500% (ISO 527 / ASTM D-638)
- Rockwell Hardness: 100 R scale (ISO 2039 / ASTM D-785)
- Flexural Modulus: 12,000 kg/cm² / 1,177 MPa (ISO 178 / ASTM D-790)
- IZOD Impact Strength, Notched, 23°C: 12 kg·cm/cm / 118 J/m (ISO 180 / ASTM D-256)
- IZOD Impact Strength, Notched, -20°C: 4.5 kg·cm/cm / 44 J/m (ISO 180 / ASTM D-256)
Thermal Properties
- Heat Deflection Temperature: 105°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 140°C (ISO 306)
Flame Characteristics
- UL Flammability Rating: UL 94HB (UL Certification)
Processing Parameters
- Melt Index: 8.5 g/10 min (ISO 1133 / ASTM D-1238)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Certifications & Compliance
- FDA Food Contact Compliance: 21 CFR 177.1520 for direct food contact
Use & Applications
- Automotive parts
- Electric appliance parts
- Battery case
- Furniture