Plastic Granules
YUNGSOX® PP 3080P Impact Copolymer
YUNGSOX® PP 3080P is an impact copolymer PP resin for protective film and CPP film. It offers 7.5 g/10 min melt flow, medium impact strength, low fish eye level, and excellent heat-sealing performance.
Associated Documents
TDS - Data Sheet
SDS - PP Impact Copolymer
BPA - PP Impact Copolymer
Haolgen - PP Impact Copolymer
PAHs - PP Impact Copolymer
REACH SVHC - PP Impact Copolymer
RoHS - PP Impact Copolymer
EN71-3 - PP Impact Copolymer
EU10-2011 - PP Impact Copolymer
FDA - PP Impact Copolymer
GB4806.6 - PP Impact Copolymer
Typical property data
Physical Properties
- Melt Index: 7.5 g/10 min (ISO 1133 / ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 260 kg/cm² / 25 MPa (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 500% (ISO 527 / ASTM D-638)
- Flexural Modulus: 12,000 kg/cm² / 1,177 MPa (ISO 178 / ASTM D-790)
- Rockwell Hardness: 93 R Scale (ISO 2039 / ASTM D-785)
- IZOD Impact Strength at 23°C: 8 kg·cm/cm Notch / 78 J/m (ISO 180 / ASTM D-256)
- IZOD Impact Strength at -20°C: 5 kg·cm/cm Notch / 49 J/m (ISO 180 / ASTM D-256)
Thermal Properties
- Heat Deflection Temperature: 108°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 152°C (ISO 306)
Processing Parameters
- Melt Index: 7.5 g/10 min (ISO 1133 / ASTM D-1238)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
- Excellent process stability
- Fish Eye Level: Low fish eye level
- Excellent heat-sealing strength
Use & Applications
- Protective film
- CPP film