Plastic Granules
YUNGSOX® PP 3084H Impact Copolymer
YUNGSOX® PP 3084H is an impact copolymer PP resin for heat-resistant and rigid molded parts. It offers 8.5 g/10 min melt index, 130°C HDT, 155°C Vicat softening point, and medium impact strength for appliances, automotive parts, and battery cases.
Associated Documents
TDS - Data Sheet
SDS - PP Impact Copolymer
BPA - PP Impact Copolymer
Haolgen - PP Impact Copolymer
PAHs - PP Impact Copolymer
REACH SVHC - PP Impact Copolymer
RoHS - PP Impact Copolymer
EN71-3 - PP Impact Copolymer
EU10-2011 - PP Impact Copolymer
FDA - PP Impact Copolymer
GB4806.6 - PP Impact Copolymer
Typical property data
Physical Properties
- Melt Index: 8.5 g/10 min (ISO 1133 / ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 290 kg/cm² / 28 MPa (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 200% (ISO 527 / ASTM D-638)
- Rockwell Hardness: 105 R scale (ISO 2039 / ASTM D-785)
- Flexural Modulus: 14,000 kg/cm² / 1,373 MPa (ISO 178 / ASTM D-790)
- IZOD Impact Strength at 23°C: 15 kg·cm/cm notch / 147 J/m (ISO 180 / ASTM D-256)
- IZOD Impact Strength at -20°C: 4.5 kg·cm/cm notch / 44 J/m (ISO 180 / ASTM D-256)
Thermal Properties
- Heat Deflection Temperature: 130°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 155°C (ISO 306)
Flame Characteristics
- UL Flame Rating: UL 94HB
- Relative Thermal Index: RTI 125°C (UL 746B)
Processing Parameters
- Melt Index for Processing Reference: 8.5 g/10 min (ISO 1133 / ASTM D-1238)
- Mold Shrinkage for Tooling Design: 1.3–1.7% (FPC Method)
Certifications & Compliance
- FDA Food Contact Compliance: 21 CFR 177.1520 for direct food contact
Use & Applications
- Electric appliance parts
- Automotive parts
- Battery case