YUNGSOX® PP 3090 Impact Copolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 3090 Impact Copolymer

YUNGSOX® PP 3090 is an impact copolymer PP resin with 8.5 g/10 min melt index and 490 J/m notched impact at 23°C. It offers balanced flow, toughness, and heat resistance for automotive parts, appliances, battery cases, and furniture.

Associated Documents

TDS - Data Sheet
SDS - PP Impact Copolymer
BPA - PP Impact Copolymer
Haolgen - PP Impact Copolymer
PAHs - PP Impact Copolymer
REACH SVHC - PP Impact Copolymer
RoHS - PP Impact Copolymer
EN71-3 - PP Impact Copolymer
EU10-2011 - PP Impact Copolymer
FDA - PP Impact Copolymer
GB4806.6 - PP Impact Copolymer

Typical property data

Physical Properties
  • Melt Index: 8.5 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 280 kg/cm² / 27 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 500% (ISO 527 / ASTM D-638)
  • Rockwell Hardness: R100 (ISO 2039 / ASTM D-785)
  • Flexural Modulus: 11,500 kg/cm² / 1,128 MPa (ISO 178 / ASTM D-790)
  • IZOD Impact Strength, Notched, 23°C: 50 kg·cm/cm / 490 J/m (ISO 180 / ASTM D-256)
  • IZOD Impact Strength, Notched, -20°C: 8.0 kg·cm/cm / 78 J/m (ISO 180 / ASTM D-256)
Thermal Properties
  • Heat Deflection Temperature: 110°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 145°C (ISO 306)
Certifications & Compliance
  • FDA Food Contact Compliance: FDA 21 CFR 177.1520 requirements for direct food contact

Use & Applications

  • Automotive parts
  • Electric appliance parts
  • Battery case
  • Furniture