Plastic Granules
YUNGSOX® PP 3155 Impact Copolymer
YUNGSOX® PP 3155 is an impact copolymer polypropylene resin for automotive parts, appliances, furniture, and luggage. It offers high gloss, anti-stress whitening, 15 g/10 min melt index, 400% elongation, and strong notched Izod impact performance.
Associated Documents
TDS - Data Sheet
SDS - PP Impact Copolymer
BPA - PP Impact Copolymer
Haolgen - PP Impact Copolymer
PAHs - PP Impact Copolymer
REACH SVHC - PP Impact Copolymer
RoHS - PP Impact Copolymer
EN71-3 - PP Impact Copolymer
EU10-2011 - PP Impact Copolymer
FDA - PP Impact Copolymer
GB4806.6 - PP Impact Copolymer
Typical property data
Physical Properties
- Melt Index: 15 g/10 min (ISO 1133 / ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 250 kg/cm² / 25 MPa (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 400% (ISO 527 / ASTM D-638)
- Flexural Modulus: 11,500 kg/cm² / 1,128 MPa (ISO 178 / ASTM D-790)
- Rockwell Hardness: 95 R scale (ISO 2039 / ASTM D-785)
- Izod Impact Strength, Notched, 23°C: 12 kg·cm/cm / 118 J/m (ISO 180 / ASTM D-256)
- Izod Impact Strength, Notched, -20°C: 6 kg·cm/cm / 59 J/m (ISO 180 / ASTM D-256)
Thermal Properties
- Heat Deflection Temperature: 105°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 140°C (ISO 306)
Optical Properties
- Gloss Performance: High gloss
- Surface Appearance: Anti-stress whitening performance
Certifications & Compliance
- DA Food Contact Compliance: FDA 21 CFR 177.1520 requirements for direct food contact