YUNGSOX® PP 3200W Impact Copolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 3200W Impact Copolymer

YUNGSOX® PP 3200W is an impact copolymer PP resin for high-gloss molded parts. It offers 20 g/10 min melt flow, 40 kg·cm/cm IZOD impact at 23°C, and 500% elongation. Use it for luggage, automotive parts, and furniture requiring flow, toughness, and surface quality.

Associated Documents

TDS - Data Sheet
SDS - PP Impact Copolymer
BPA - PP Impact Copolymer
Haolgen - PP Impact Copolymer
PAHs - PP Impact Copolymer
REACH SVHC - PP Impact Copolymer
RoHS - PP Impact Copolymer
EN71-3 - PP Impact Copolymer
EU10-2011 - PP Impact Copolymer
FDA - PP Impact Copolymer
GB4806.6 - PP Impact Copolymer

Typical property data

Physical Properties
  • Melt Index: 20 g/10 min (ISO 1133)
  • Density: 0.90 g/cm³ (ISO 1183)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 250 kg/cm² (ISO 527)
  • Tensile Elongation at Break: 500% (ISO 527)
  • Flexural Modulus: 8,000 kg/cm² (ISO 178)
  • Rockwell Hardness: 100 R scale (ISO 2039)
  • IZOD Impact Strength, Notched, 23°C: 40 kg·cm/cm (ISO 180)
  • IZOD Impact Strength, Notched, -20°C: 6.5 kg·cm/cm (ISO 180)
Thermal Properties
  • Heat Deflection Temperature: 100°C (ISO 75)
  • Vicat Softening Temperature: 135°C (ISO 306)
Optical Properties
  • High Gloss
Processing Parameters
  • Recommended Processing Method: Injection molding application
  • Melt Index for Processing Reference: 20 g/10 min (ISO 1133)
  • Mold Shrinkage for Tooling Reference: 1.3–1.7% (FPC Method)
Certifications & Compliance
  • FDA Food Contact Compliance: FDA 21 CFR 177.1520

Use & Applications

  • Luggage
  • Automotive parts
  • Furniture