YUNGSOX® PP 3354 Impact Copolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 3354 Impact Copolymer High Fluidity

YUNGSOX® PP 3354 is an impact copolymer PP resin with high fluidity and medium impact strength. It has a 35 g/10 min melt index, 0.90 g/cm³ density, and FDA food contact compliance. Ideal for large automotive parts, appliances, tool boxes, and thin-wall products.

Associated Documents

TDS - Data Sheet
PL JCII Certification
SDS - PP Impact Copolymer
BPA - PP Impact Copolymer
Haolgen - PP Impact Copolymer
PAHs - PP Impact Copolymer
REACH SVHC - PP Impact Copolymer
RoHS - PP Impact Copolymer
EN71-3 - PP Impact Copolymer
EU10-2011 - PP Impact Copolymer
FDA - PP Impact Copolymer
GB4806.6 - PP Impact Copolymer

Typical property data

Physical Properties
  • Melt Index: 35 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 250 kg/cm² / 25 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 100% (ISO 527 / ASTM D-638)
  • Rockwell Hardness: 95 R scale (ISO 2039 / ASTM D-785)
  • Flexural Modulus: 12,500 kg/cm² / 1,226 MPa (ISO 178 / ASTM D-790)
  • IZOD Impact Strength at 23°C: 9 kg·cm/cm Notch / 88 J/m (ISO 180 / ASTM D-256)
  • IZOD Impact Strength at -20°C: 4 kg·cm/cm Notch / 39 J/m (ISO 180 / ASTM D-256)
Thermal Properties
  • Heat Deflection Temperature: 105°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 140°C (ISO 306)
Processing Parameters
  • Flow Characteristic: High fluidity
  • Medium impact strength
  • Mold Shrinkage: 1.3–1.7% (FPC Method)

Use & Applications

  • Larger automotive parts
  • Electric appliance parts
  • Washing machine parts
  • Tool boxes
  • Storage boxes
  • Thin-wall products