YUNGSOX® PP 4084 Impact Copolymer
YUNGSOX® PP 4084 is an impact copolymer PP resin for tough molded parts. It offers high impact strength, excellent low-temperature brittleness resistance, 10 g/10 min melt index, and FDA 21 CFR 177.1520 food contact compliance for reliable pp plastic raw material sourcing.
Associated Documents
TDS - Data Sheet
SDS - PP Impact Copolymer
BPA - PP Impact Copolymer
Haolgen - PP Impact Copolymer
PAHs - PP Impact Copolymer
REACH SVHC - PP Impact Copolymer
RoHS - PP Impact Copolymer
EN71-3 - PP Impact Copolymer
EU10-2011 - PP Impact Copolymer
FDA - PP Impact Copolymer
GB4806.6 - PP Impact Copolymer
Typical property data
Physical Properties
- Melt Index: 10 g/10 min (ISO 1133 / ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 220 kg/cm² / 22 MPa (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 550% (ISO 527 / ASTM D-638)
- Flexural Modulus: 9,000 kg/cm² / 883 MPa (ISO 178 / ASTM D-790)
- Rockwell Hardness: 95 R scale (ISO 2039 / ASTM D-785)
- IZOD Impact Strength, Notched, 23°C: 40 kg·cm/cm / 392 J/m (ISO 180 / ASTM D-256)
- IZOD Impact Strength, Notched, -20°C: 10 kg·cm/cm / 98 J/m (ISO 180 / ASTM D-256)
Thermal Properties
- Heat Deflection Temperature: 100°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 135°C (ISO 306)
Processing Parameters
- Melt Index: 10 g/10 min (ISO 1133 / ASTM D-1238)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Certifications & Compliance
- FDA Food Contact Compliance: FDA 21 CFR 177.1520
Use & Applications
- Bumpers
- Automotive parts
- Heavy duty container
- Pallet