YUNGSOX® PP 4204 Impact Copolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 4204 Impact Copolymer

YUNGSOX® PP 4204 is an impact copolymer PP resin for injection molding. It offers 19 g/10 min melt flow, high impact strength, and strong low-temperature toughness. Ideal for bumpers, automotive parts, pallets, and heavy-duty containers.

Associated Documents

TDS - Data Sheet
SDS - PP Impact Copolymer
BPA - PP Impact Copolymer
Haolgen - PP Impact Copolymer
PAHs - PP Impact Copolymer
REACH SVHC - PP Impact Copolymer
RoHS - PP Impact Copolymer
EN71-3 - PP Impact Copolymer
EU10-2011 - PP Impact Copolymer
FDA - PP Impact Copolymer
GB4806.6 - PP Impact Copolymer

Typical property data

Physical Properties
  • Melt Index: 19 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 210 kg/cm² / 21 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 550% (ISO 527 / ASTM D-638)
  • Flexural Modulus: 9,500 kg/cm² / 932 MPa (ISO 178 / ASTM D-790)
  • Rockwell Hardness: 92 R scale (ISO 2039 / ASTM D-785)
  • IZOD Impact Strength at 23°C: 50 kg·cm/cm Notch / 490 J/m (ISO 180 / ASTM D-256)
  • IZOD Impact Strength at -20°C: 10 kg·cm/cm Notch / 98 J/m (ISO 180 / ASTM D-256)
Thermal Properties
  • Heat Deflection Temperature: 100°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 135°C (ISO 306)
Certifications & Compliance
  • FDA Food Contact Compliance: 21 CFR 177.1520 for direct food contact

Use & Applications

  • Bumpers
  • Automotive parts
  • Heavy duty container