YUNGSOX® PP 5003 Random Copolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 5003 Random Copolymer For PP-R Pipe

YUNGSOX® PP 5003 is a Random Copolymer PP resin for PP-R pipe, thermoforming sheet, and blow molding. It offers 0.25 g/10 min MI, 500% elongation, high impact strength, creep resistance, and FDA food-contact compliance. Good for drinking water pipe applications.

Associated Documents

TDS - Data Sheet
PPR copolymer - Halogen
PPR copolymer - PAHs
PPR copolymer - REACH SVHC
PPR copolymer - RoHS
PPR copolymer - BPA
PPR copolymer - EN71-3
PPR copolymer - EU10-2011
PPR copolymer - FDA
PP Terpolymer - EU10-2011

Typical property data

Physical Properties
  • Melt Index: 0.25 g/10 min (ISO 1133)
  • Density: 0.90 g/cm³ (ISO 1183)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 250 kg/cm² (ISO 527)
  • Tensile Elongation at Break: 500% (ISO 527)
  • Flexural Modulus: 8,000 kg/cm² (ISO 178)
  • Rockwell Hardness: 90 R scale (ISO 2039)
  • IZOD Impact Strength at 23°C: 40 kg·cm/cm, notched (ISO 180)
  • IZOD Impact Strength at -20°C: 6 kg·cm/cm, notched (ISO 180)
Thermal Properties
  • Melting Point: 142°C (DSC)
  • Heat Deflection Temperature: 85°C (ISO 75)
  • Vicat Softening Temperature: 128°C (ISO 306)
Processing Performance
  • Excellent creep resistance for long-term pipe service
  • Good low-temperature brittleness resistance for cold-environment use
  • High impact strength for pipe and molded part durability
  • Excellent whitening resistance for stress-whitening control
Certifications & Compliance
  • FDA Food Contact Compliance: FDA 21 CFR 177.1520 requirements for food contact

Use & Applications

  • PP-R pipe for drinking water, waste systems, and under-floor heating circuits
  • Thermoforming sheet
  • Blow molding