Yungsox PP 5003 Polypropylene Transparent Particles PPR Blow Molding
YUNGSOX 5003, manufactured by Formosa Plastics Corporation, is a high-performance Random Copolymer Polypropylene (PP-R) resin ideal for pipe extrusion and blow molding. Engineered for demanding industrial and commercial applications, it offers exceptional impact resistance, superior creep resistance, and outstanding performance in low-temperature environments.
Associated Documents
TDS - Data Sheet
Typical property data
Physical Properties
- Melt Index: 0.25 g/10min (ISO 1133)
- Density: 0.90 g/cm³ (ISO 1183)
Mechanical Properties
- Tensile Strength at Yield: 250 Kg/cm² (ISO 527)
- Tensile Elongation at Break: 500% (ISO 527)
- Rockwell Hardness: R scale 90 (ISO 2039)
- Flexural Modulus: 8,000 Kg/cm² (ISO 178)
- IZOD Impact Strength:
- 23℃: 40 Kg.cm/cm (ISO 180)
- -20℃: 6 Kg.cm/cm (ISO 180)
Thermal Properties
- Melting Point: 142℃ (DSC)
- Heat Deflection Temperature: 85℃ (ISO 75)
- Vicat Softening Temperature: 128℃ (ISO 306)
Optical Properties
- Yellowing Index: 20 (HG/T 3862-2006)
- Whiteness: 64% (GB/T 2913-1982)
Processing Parameters
- Mold Shrinkage: 1.3%-1.7% (FPC Method)
Additional Certifications
- FDA Approval: Complies with FDA 21 CFR 177.1520 for food contact applications.
Use & Applications
- PP-R pipe for drinking water
- waste system
- under-floor heating circuits
- Thermoforming sheet
- Blow molding