YUNGSOX® PP 5018 Random Copolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 5018 Random Copolymer

YUNGSOX® PP 5018 is a random copolymer PP resin for blow-molded pharmaceutical bottles. It offers 1.7 g/10 min melt index, 500% elongation, and good chemical resistance. FDA 21 CFR 177.1520 and USP Class VI compliance support regulated packaging use.

Associated Documents

TDS - Data Sheet
USP Class VI
PPR copolymer - Halogen
PPR copolymer - PAHs
PPR copolymer - REACH SVHC
PPR copolymer - RoHS
PPR copolymer - BPA
PPR copolymer - EN71-3
PPR copolymer - EU10-2011
PPR copolymer - FDA
PP Terpolymer - EU10-2011

Typical property data

Physical Properties
  • Melt Index: 1.7 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 250 kg/cm² / 25 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 500% (ISO 527 / ASTM D-638)
  • Rockwell Hardness: 90 R scale (ISO 2039 / ASTM D-785)
  • Flexural Modulus: 9,500 kg/cm² / 932 MPa (ISO 178 / ASTM D-790)
  • IZOD Impact Strength, Notched, 23°C: 8 kg·cm/cm / 78 J/m (ISO 180 / ASTM D-256)
Thermal Properties
  • Melting Point: 146°C (DSC)
  • Heat Deflection Temperature: 90°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 120°C (ISO 306)
Processing Parameters
  • Recommended Processing Method: Blow molding
  • Melt Index for Processing Reference: 1.7 g/10 min (ISO 1133 / ASTM D-1238)
  • Mold Shrinkage for Tooling Design: 1.3–1.7% (FPC Method)
  • Typical Application Processing Fit: Pharmaceutical bottle blow molding
  • Chemical Resistance: Good resistance to chemical
Certifications & Compliance
  • FDA Food Contact Compliance: 21 CFR 177.1520 requirements for direct food contact
  • USP Biological Reactivity: USP Plastic Class VI requirements

Use & Applications

  • Blow molding
  • Pharmaceutical bottle
fpc taiwan polypropylene pp resin 25kg package

Send Us a Message