YUNGSOX® PP 5050 Random Copolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 5050 Random Copolymer

YUNGSOX® PP 5050 is a terpolymer PP resin for heat sealing layers and shrink films. It offers low heat seal temperature, good softness, 500% elongation, <1.0% haze, and FDA 21 CFR 177.1520 food contact compliance.

Associated Documents

TDS - Data Sheet
JCII PL Test
PPR copolymer - Halogen
PPR copolymer - PAHs
PPR copolymer - REACH SVHC
PPR copolymer - RoHS
PPR copolymer - BPA
PPR copolymer - EN71-3
PPR copolymer - EU10-2011
PPR copolymer - FDA
PP Terpolymer - EU10-2011

Typical property data

Physical Properties
  • Melt Index: 6.5 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.0–1.2% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 200 kg/cm² / 20 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 500% (ISO 527 / ASTM D-638)
  • Flexural Modulus: 5,000 kg/cm² / 490 MPa (ISO 178 / ASTM D-790)
  • Rockwell Hardness: 80 R scale (ISO 2039 / ASTM D-785)
  • IZOD Impact Strength, Notched, 23°C: 10 kg·cm/cm / 98 J/m (ISO 180 / ASTM D-256)
Thermal Properties
  • Melting Point: 132°C (DSC)
  • Heat Deflection Temperature: 75°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 110°C (ISO 306)
Optical Properties
  • Haze, 30 μm Film: < 1.0% (FPC Method)
Certifications & Compliance
  • FDA Food Contact Compliance: 21 CFR 177.1520 for direct food contact

Use & Applications

  • Heat sealing layer
  • Shrink film
fpc taiwan polypropylene pp resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.