YUNGSOX® PP 5050M Random Copolymer
YUNGSOX® PP 5050M is a random copolymer PP resin for aluminum metallized cast film and heat sealing layers. It offers low heat seal temperature, good softness, and excellent laminate processing, with 6.5 g/10 min MI and <1.5% haze.
Associated Documents
TDS - Data Sheet
USP Class VI
PPR copolymer - Halogen
PPR copolymer - PAHs
PPR copolymer - REACH SVHC
PPR copolymer - RoHS
PPR copolymer - BPA
PPR copolymer - EN71-3
PPR copolymer - EU10-2011
PPR copolymer - FDA
PP Terpolymer - EU10-2011
Typical property data
Physical Properties
- Melt Index: 6.5 g/10 min (ISO 1133 / ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
- Mold Shrinkage: 1.0–1.2% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 200 kg/cm² / 20 MPa (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 500% (ISO 527 / ASTM D-638)
- Flexural Modulus: 5,500 kg/cm² / 539 MPa (ISO 178 / ASTM D-790)
- Rockwell Hardness: 85 R scale (ISO 2039 / ASTM D-785)
- IZOD Impact Strength at 23°C: 10 kg·cm/cm Notch / 98 J/m (ISO 180 / ASTM D-256)
Thermal Properties
- Melting Point: 131°C (DSC)
- Heat Deflection Temperature: 80°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 110°C (ISO 306)
Optical Properties
- Haze at 30 μm Film Thickness: < 1.5% (FPC Method)
Certifications & Compliance
- FDA Food Contact Compliance: FDA 21 CFR 177.1520 requirements for direct food contact
- USP Biological Reactivity: USP Plastic Class VI requirements
Use & Applications
- Aluminum metallized cast film
- heat sealing layer