YUNGSOX® PP 5050R Random Copolymer
YUNGSOX® PP 5050R is a terpolymer PP resin for heat sealing layer and shrink film. It offers low heat seal temperature, good softness, 6.5 g/10 min melt index, <0.6% haze in 30 μm film, and FDA food contact compliance.
Associated Documents
TDS - Data Sheet
JCII PL Test
PPR copolymer - Halogen
PPR copolymer - PAHs
PPR copolymer - REACH SVHC
PPR copolymer - RoHS
PPR copolymer - BPA
PPR copolymer - EN71-3
PPR copolymer - EU10-2011
PPR copolymer - FDA
PP Terpolymer - EU10-2011
Typical property data
Physical Properties
- Melt Index: 6.5 g/10 min (ISO 1133 / ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
- Mold Shrinkage: 1.0–1.2% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 200 kg/cm² / 20 MPa (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 500% (ISO 527 / ASTM D-638)
- Flexural Modulus: 5,000 kg/cm² / 490 MPa (ISO 178 / ASTM D-790)
- Rockwell Hardness: 80 R scale (ISO 2039 / ASTM D-785)
- IZOD Impact Strength, Notched at 23°C: 10 kg·cm/cm / 98 J/m (ISO 180 / ASTM D-256)
Thermal Properties
- Melting Point: 130°C (DSC)
- Heat Deflection Temperature: 75°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 110°C (ISO 306)
- Heat Seal Performance Indicator: Low heat seal temperature
Optical Properties
- Haze, 30 μm Film: < 0.6% (FPC Method)
Certifications & Compliance
- FDA Food Contact Compliance: 21 CFR 177.1520 for direct food contact
Use & Applications
- Heat sealing layer film
- shrink film