Plastic Granules
YUNGSOX® PP 5060 Random Copolymer
YUNGSOX® PP 5060 is a random copolymer PP resin for ISBM pharmaceutical bottles. It offers good chemical resistance, 7 g/10 min melt index, 500% elongation, and FDA 21 CFR 177.1520 food-contact compliance for reliable packaging.
Associated Documents
TDS - Data Sheet
USP Class VI
PPR copolymer - Halogen
PPR copolymer - PAHs
PPR copolymer - REACH SVHC
PPR copolymer - RoHS
PPR copolymer - BPA
PPR copolymer - EN71-3
PPR copolymer - EU10-2011
PPR copolymer - FDA
PP Terpolymer - EU10-2011
Typical property data
Physical Properties
- Melt Index: 7 g/10 min (ISO 1133 / ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 270 kg/cm² / 26 MPa (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 500% (ISO 527 / ASTM D-638)
- Rockwell Hardness: 95 R scale (ISO 2039 / ASTM D-785)
- Flexural Modulus: 9,000 kg/cm² / 883 MPa (ISO 178 / ASTM D-790)
- IZOD Impact Strength at 23°C: 4.5 kg·cm/cm notch / 44 J/m (ISO 180 / ASTM D-256)
Thermal Properties
- Melting Point: 146°C (DSC)
- Heat Deflection Temperature: 90°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 125°C (ISO 306)
Processing Performance
- Recommended Processing: ISBM
- Melt Index: 7 g/10 min (ISO 1133 / ASTM D-1238)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Certifications & Compliance
- FDA Food Contact Compliance: FDA 21 CFR 177.1520 for direct food contact
- USP Biological Reactivity: USP Plastic Class VI requirements.
Use & Applications
- ISBM
- Pharmaceutical bottle