Plastic Granules
YUNGSOX® PP 5090R Random Copolymer
YUNGSOX® PP 5090R is a high-transparency random copolymer PP resin for medical and food-contact parts. It offers a 19 g/10 min melt index, γ-ray sterilization resistance, chemical resistance, and 10% energy-saving production.
Associated Documents
TDS - Data Sheet
USP Class VI
ISO 10993
PPR copolymer - Halogen
PPR copolymer - PAHs
PPR copolymer - REACH SVHC
PPR copolymer - RoHS
PPR copolymer - BPA
PPR copolymer - EN71-3
PPR copolymer - EU10-2011
PPR copolymer - FDA
PP Terpolymer - EU10-2011
Typical property data
Physical Properties
- Melt Index: 19 g/10 min (ISO 1133 / ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 280 kg/cm² / 27 MPa (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 300% (ISO 527 / ASTM D-638)
- Flexural Modulus: 10,500 kg/cm² / 1,030 MPa (ISO 178 / ASTM D-790)
- Rockwell Hardness: 98, R scale (ISO 2039 / ASTM D-785)
- IZOD Impact Strength, Notched, 23°C: 6 kg·cm/cm / 59 J/m (ISO 180 / ASTM D-256)
Thermal Properties
- Melting Point: 146°C (DSC)
- Heat Deflection Temperature: 95°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 125°C (ISO 306)
Optical Properties
- High transparency
- Optical Application Relevance: PP parts requiring transparent medical and food-contact components
Processing Parameters
- Sterilization Compatibility: Suitable for γ-ray sterilization / Anti γ-ray
- Chemical Resistance: Good resistance to chemicals
- Energy-Saving Processing Benefit: Average 10% energy saving for production of clarified PP parts
Certifications & Compliance
- FDA Food Contact Compliance: 21 CFR 177.1520 for direct food contact
- USP Biological Reactivity: USP Plastic Class VI requirements
- ISO 10993 Biocompatibility
Use & Applications
- Disposable syringes
- Anti γ ray