Plastic Granules
YUNGSOX® PP 5090T Random Copolymer High Transparency
YUNGSOX® PP 5090T is a random copolymer PP resin for clear molded products. It offers high transparency, good chemical resistance, 15 g/10 min melt flow, and FDA, USP Class VI, and UL 94HB compliance for containers, housewares, and disposable syringes.
Associated Documents
TDS - Data Sheet
USP Class VI
JCII PL Test
PPR copolymer - Halogen
PPR copolymer - PAHs
PPR copolymer - REACH SVHC
PPR copolymer - RoHS
PPR copolymer - BPA
PPR copolymer - EN71-3
PPR copolymer - EU10-2011
PPR copolymer - FDA
PP Terpolymer - EU10-2011
Typical property data
Physical Properties
- Melt Index: 15 g/10 min (ISO 1133 / ASTM D-1238)
- Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 280 kg/cm² / 27 MPa (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 300% (ISO 527 / ASTM D-638)
- Flexural Modulus: 10,500 kg/cm² / 1,030 MPa (ISO 178 / ASTM D-790)
- IZOD Impact Strength, Notched, 23°C: 6 kg·cm/cm / 59 J/m (ISO 180 / ASTM D-256)
- IZOD Impact Strength, Notched, -20°C: — (ISO 180 / ASTM D-256)
- Rockwell Hardness: 98 R scale (ISO 2039 / ASTM D-785)
Thermal Properties
- Melting Point: 146°C (DSC)
- Heat Deflection Temperature: 95°C (ISO 75 / ASTM D-648)
- Vicat Softening Temperature: 125°C (ISO 306)
Flame Characteristics
- UL Flammability Rating: UL 94HB (UL 94)
Certifications & Compliance
- FDA Food Contact Compliance: FDA 21 CFR 177.1520 for direct food contact
- USP Biological Reactivity: USP Plastic Class VI requirements
- UL Certification: UL 94HB
Use & Applications
- High transparency containers
- Transparent housewares
- Disposable syringes