YUNGSOX® PP 5200XT is a random copolymer PP resin for clear molded parts. It offers high transparency, good chemical resistance, and FDA food-contact compliance. Its 18 g/10 min melt index supports stable processing, with 10% average energy savings.

Associated Documents

TDS - Data Sheet
PPR copolymer - Halogen
PPR copolymer - PAHs
PPR copolymer - REACH SVHC
PPR copolymer - RoHS
PPR copolymer - BPA
PPR copolymer - EN71-3
PPR copolymer - EU10-2011
PPR copolymer - FDA
PP Terpolymer - EU10-2011

Typical property data

Physical Properties
  • Melt Index: 18 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 280 kg/cm² / 27 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 300% (ISO 527 / ASTM D-638)
  • Flexural Modulus: 10,500 kg/cm² / 1,030 MPa (ISO 178 / ASTM D-790)
  • Rockwell Hardness: 98 R scale (ISO 2039 / ASTM D-785)
  • IZOD Impact Strength, Notched, 23°C: 6 kg·cm/cm / 59 J/m (ISO 180 / ASTM D-256)
Thermal Properties
  • Melting Point: 146°C (DSC)
  • Heat Deflection Temperature: 95°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 125°C (ISO 306)
Optical Properties
  • High transparency
Processing Parameters
  • Melt Index: 18 g/10 min (ISO 1133 / ASTM D-1238)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
  • Energy-Saving Processing Claim: Average 10% energy savings for production of clarified PP parts
Certifications & Compliance
  • FDA Food Contact Compliance: 21 CFR 177.1520 requirements for direct food contact
  • UL Environment Claim Validation Mark:
    an average 10% energy saving for production of clarified PP parts

Use & Applications

  • High transparency containers
  • transparent housewares
  • disposable syringes