YUNGSOX® PP 5350T Random Copolymer

fpc taiwan polypropylene pp resin 25kg package

YUNGSOX® PP 5350T Random Copolymer

YUNGSOX® PP 5350T is a random copolymer PP resin for clear molded parts. It offers high fluidity, high transparency, and good chemical resistance. With FDA, USP Class VI, JHOSPA-PL, and UL 94HB compliance, it fits containers, housewares, and syringes.

Associated Documents

TDS - Data Sheet
USP Class VI
JCII PL Test
PPR copolymer - Halogen
PPR copolymer - PAHs
PPR copolymer - REACH SVHC
PPR copolymer - RoHS
PPR copolymer - BPA
PPR copolymer - EN71-3
PPR copolymer - EU10-2011
PPR copolymer - FDA
PP Terpolymer - EU10-2011

Typical property data

Physical Properties
  • Melt Index: 35 g/10 min (ISO 1133 / ASTM D-1238)
  • Density: 0.90 g/cm³ (ISO 1183 / ASTM D792)
  • Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
  • Tensile Strength at Yield: 280 kg/cm² / 27 MPa (ISO 527 / ASTM D-638)
  • Tensile Elongation at Break: 200% (ISO 527 / ASTM D-638)
  • Flexural Modulus: 10,500 kg/cm² / 1,030 MPa (ISO 178 / ASTM D-790)
  • Rockwell Hardness: 98, R scale (ISO 2039 / ASTM D-785)
  • IZOD Impact Strength, Notched, 23°C: 5 kg·cm/cm / 49 J/m (ISO 180 / ASTM D-256)
Thermal Properties
  • Melting Point: 146°C (DSC)
  • Heat Deflection Temperature: 95°C (ISO 75 / ASTM D-648)
  • Vicat Softening Temperature: 125°C (ISO 306)
Optical Properties
  • High transparency Performance
Flame Characteristics
  • Flame Characteristics
Processing Parameters
  • Flow Performance: High fluidity supported by 35 g/10 min Melt Index (ISO 1133 / ASTM D-1238)
  • Processing Benefit: Average 10% energy savings for production of clarified PP parts
Certifications & Compliance
  • FDA Food Contact Compliance: 21 CFR 177.1520 for direct food contact
  • UL Certification: UL 94HB, UL file no. E216959
  • USP Biological Reactivity: USP Plastic Class VI
  • JHOSPA-PL Certification: Certified to JHOSPA-PL requirements
  • UL Environment Claim Validation Mark: Validated for average 10% energy savings in clarified PP part production

Use & Applications

  • High-transparency containers
  • transparent housewares
  • disposable syringes