Plastic Granules
YUNGSOX® PP 5450XT Random Copolymer
YUNGSOX® PP 5450XT is a random copolymer PP resin for clear containers, housewares, and food-contact products. It offers high fluidity, high transparency, good chemical resistance, and FDA 21 CFR 177.1520 compliance for direct food contact.
Associated Documents
TDS - Data Sheet
PPR copolymer - Halogen
PPR copolymer - PAHs
PPR copolymer - REACH SVHC
PPR copolymer - RoHS
PPR copolymer - BPA
PPR copolymer - EN71-3
PPR copolymer - EU10-2011
PPR copolymer - FDA
PP Terpolymer - EU10-2011
Typical property data
Physical Properties
- Melt Index: 45 g/10 min (ISO 1133)
- Density: 0.90 g/cm³ (ISO 1183)
- Mold Shrinkage: 1.3–1.7% (FPC Method)
Mechanical Properties
- Tensile Strength at Yield: 280 kg/cm² (ISO 527)
- Tensile Elongation at Break: 600% (ISO 527)
- Flexural Modulus: 10,000 kg/cm² (ISO 178)
- Rockwell Hardness: 90 R scale (ISO 2039)
- IZOD Impact Strength, Notched, 23°C: 4.5 kg·cm/cm (ISO 180)
Thermal Properties
- Heat Deflection Temperature: 95°C (ISO 75)
Optical Properties
- High Transparency Performance
Processing Performance
- High-Flow Processing Indicator: Melt Index 45 g/10 min (ISO 1133)
- Mold Shrinkage Range: 1.3–1.7% (FPC Method)
- Processing Characteristic: High fluidity
Certifications & Compliance
- FDA Food Contact Compliance: FDA 21 CFR 177.1520 for direct food contact
Use & Applications
- Injection-molded transparent containers
- housewares
- food containers