Plastic Granules
YUNGSOX® PP 6020P Homopolymer
YUNGSOX® PP 6020P is a homopolymer polypropylene resin designed for separator and microporous membrane applications. It offers superior mechanical performance and processing ease, ideal for high-strength and durable solutions. Characteristics: Excellent tensile strength, Excellent puncture strength, Good porosity.
Associated Documents
TDS - Data Sheet
SDS - PPH
BPA - PPH
Haolgen - PPH
PAHs - PPH
REACH SVHC - PPH
RoHS - PPH
EN71-3 - PPH
EU10-2011 - PPH
FDA - PPH
GB4806.6 - PPH
Typical property data
Physical Properties
- Melt Index: 2.0 g/10 min (ISO 1133 / ASTM D-1238)
Mechanical Properties
- Tensile Strength at Yield: 370 kg/cm² (36 MPa) (ISO 527 / ASTM D-638)
- Tensile Elongation at Break: 600% (ISO 527 / ASTM D-638)
- Flexural Modulus: 16,500 kg/cm² (1618 MPa) (ISO 178 / ASTM D-790)
- IZOD Impact Strength (Notched):
- At 23°C: 4.5 kg·cm/cm (44 J/m) (ISO 180 / ASTM D-256)
- At -20°C: Not provided
- Rockwell Hardness: 112 (R-scale) (ISO 2039 / ASTM D-785)
Thermal Properties
- Heat Deflection Temperature: 120°C (ISO 75 / ASTM D648)
- Vicat Softening Temperature: 155°C (ISO 306)
Certifications & Compliance
- FDA Approval: Meets 21 CFR 177.1520 standards for food contact applications.
Use & Applications
- Separator films
- Microporous membranes