Yuntianhua® GF-10 POM

yuntianhua acetal copolymer pom package

Yuntianhua® GF-10 Pellets 10% Glass Fiber Acetal POM Copolymer

Yuntianhua® GF-10 is a 10% glass fiber reinforced POM copolymer for injection molding. It offers high stiffness, 90 MPa tensile yield stress, 155°C HDT, and low shrinkage. Suitable for gears, bearings, valves, cams, pedals, and other precision parts.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Density: 1.5 g/cm³ (ISO 1183)
  • Melt Mass-Flow Rate, MFR: 6 g/10 min at 190°C / 2.16 kg (ISO 1133)
  • Water Absorption: 0.6% after 24 hr at 23°C (ISO 62)
Mechanical Properties
  • Tensile Stress at Yield: 90 MPa (ISO 527-2)
  • Tensile Modulus: 4500 MPa (ISO 527-2)
  • Strain at Break: 3.5% (ISO 527-2)
  • Flexural Strength: 100 MPa (ISO 178)
  • Flexural Modulus: 4000 MPa (ISO 178)
  • Charpy Notched Impact Strength: 4.0 kJ/m² (ISO 179/1eA)
Thermal Properties
  • Heat Deflection Temperature: 155°C at 1.8 MPa, unannealed (ISO 75)
  • Claimed HDT Performance: up to 150°C according to product feature description
Flame Characteristics
  • UL Flame Rating: HB class (UL 94)
Injection Molding Conditions
  • Material Drying: 100–120°C for 2–4 hr
  • Nozzle Temperature: 180–210°C
  • Front Section Temperature: 180–210°C
  • Center Section Temperature: 170–200°C
  • Rear Section Temperature: 160–180°C
  • Melt Temperature: 180–210°C
  • Mold Temperature: 60–90°C
  • Mold Temperature for Precision Parts: Up to 120°C
  • Injection Pressure: 50–100 MPa
  • Holding Pressure: 30–80 MPa
  • Back Pressure: 0–0.5 MPa
  • Screw Rotational Speed: 50–120 rpm

Use & Applications

  • Oil box cover
  • Gear
  • Accelerator pedal
  • Radiator cover
  • Bearing
  • Conveyor belt
  • Valve
  • Cam
  • Impeller
yuntianhua acetal copolymer pom package