Zhenjiang Chimei Kibisan® D-168

zhenjiang chimei san resin as resin 25kg package

Kibisan® D-168 SAN General Grade

KIBISAN® D-168 is a robust, general-grade SAN plastic resin offering high strength, excellent chemical resistance, and versatility. Featuring easy processing and reliable mechanical properties, D-168 is ideal for demanding applications in consumer, industrial, and appliance sectors.

Associated Documents

ISO TDS - Data Sheet
ASTM TDS - Data Sheet
UL Product iQ
Processing Data
MSDS - Safety Data Sheet
REACH SVHC

Typical property data

Physical Properties
  • Density: 1.08 (ISO 1183, 23℃)
  • Melt Flow Rate (MFR): 11.0 cm³/10 min (ISO 1133, 220℃, 10 kg)
Mechanical Properties
  • Tensile Strength: 81 MPa (ISO 527, 50 mm/min)
  • Elongation at Break: 7.0% (ISO 527, 50 mm/min)
  • Flexural Strength: 124 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 3.7 GPa (ISO 178, 2 mm/min)
  • Hardness: M-85 (ASTM D785, M-Scale)
Impact Properties
  • Izod Impact Strength: 4.0 kJ/m² (ISO 180, 4 mm notch, 23℃)
Thermal Properties
  • Vicat Softening Temperature: 108℃ (ISO 306, 50℃/hr)
  • H.D.T (Heat Deflection Temperature, Unannealed): 89℃ (ISO 75-2, Unannealed)
Flame Characteristics
  • Flammability Rating: 1.5 mm HB (UL & C-UL File No. E194560)

Use & Applications

  • Toothbrush Handles
  • Lighter Shells
  • Fan Blades
zhenjiang chimei san resin as resin 25kg package

Features & Benefits

1. Superior Mechanical Performance

With a tensile strength of 81 MPa (ISO 527), KIBISAN® D-168 ensures exceptional durability for long-lasting applications.

2. Reliable Thermal Resistance

A Vicat softening point of 108℃ (ISO 306) guarantees stable performance in heat-sensitive environments and processes.

3. Enhanced Chemical Durability

Engineered for high chemical resistance, this material resists wear and tear from harsh substances, boosting product lifespan.

zhenjiang chimei san resin as resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.