Physical Properties
  • Density: 1.07 g/cm³ (ISO 1183, 23°C)
  • Melt Flow Rate (MFR): 19.0 cm³/10 min (ISO 1133, 200°C, 5 kg)
Mechanical Properties
  • Tensile Strength: 57 MPa (ISO 527, 50 mm/min)
  • Elongation at Break: 4.0% (ISO 527, 50 mm/min)
  • Flexural Strength: 75 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 3.4 GPa (ISO 178, 2 mm/min)
  • Hardness: M-74, M-Scale (ASTM D785)
Impact Properties
  • IZOD Impact Strength: 3.7 kJ/m² (ISO 180, 23°C, 4 mm)
Thermal Properties
  • Softening Point: 104°C (ISO 306, 50°C/hr)
  • Heat Deflection Temperature (HDT) – Unannealed: 85°C (ISO 75-2, Unannealed)
Flame Characteristics
  • Burning Rate: 1.5 mm HB (UL 94, File No. E194560)

Use & Applications

  • Masterbatch Substrates
  • Precise Injection Molded Components
  • Modified Material Production
zhenjiang chimei san resin as resin 25kg package

Features & Benefits

1. Exceptional High-Flow Performance

The high-flow properties ensure efficient mold filling, faster cycle times, and flawless finishes, making it ideal for intricate designs and thin-walled applications.

2. Robust Mechanical Strength

The tensile strength of 57 MPa and flexural modulus of 3.4 GPa ensure durability for products requiring long-term structural integrity, such as industrial parts and consumer goods.

3. Reliable Thermal Stability

With a softening point of 104°C and HDT of 85°C, D-178HF performs seamlessly under moderate heat, preventing deformation in electronics, packaging, and other temperature-sensitive uses.

zhenjiang chimei san resin as resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.