Kibisan® PN-108L100 SAN General Grade Natural Color

KIBISAN® PN-108L100 is a high-performance SAN (Styrene Acrylonitrile) resin, designed for versatile applications. As a general-grade, natural-colored material, it combines excellent mechanical strength, thermal stability, and an easy processing profile—ideal for Daily necessities, cosmetic cases.

Associated Documents

ISO TDS - Data Sheet
ASTM TDS - Data Sheet
UL Product iQ
Processing Data
MSDS - Safety Data Sheet
REACH SVHC

Typical property data

Physical Properties
  • Density: 1.07 (ISO 1183, at 23°C)
  • Melt Flow Rate (MFR): 5.0 cm³/10min (ISO 1133, 200°C, 5kg)
Mechanical Properties
  • Tensile Strength: 67 MPa (ISO 527, 50 mm/min)
  • Elongation: 5.0% (ISO 527, 50 mm/min)
  • Flexural Strength: 101 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 3.4 GPa (ISO 178, 2 mm/min)
  • Hardness (Rockwell): M-83 (ASTM D785, M-Scale)
Impact Properties
  • IZOD Impact Strength: 3.8 kJ/m² (ISO 180, 4 mm, 23°C)
Thermal Properties
  • Softening Point: 105°C (ISO 306, 50°C/hr)
  • Heat Deflection Temperature (HDT), Unannealed: 86°C (ISO 75-2, Unannealed)
Flame Characteristics
  • Burning Rate: HB (UL 94, 1.5 mm, File No. E194560)

Use & Applications

  • Daily Necessities
  • Cosmetic Cases
zhenjiang chimei san resin as resin 25kg package

Features & Benefits

1. Superior Mechanical Strength

It offers tensile strength of 67 MPa and flexural strength of 101 MPa for robust, long-lasting components.

2. Reliable Thermal Performance

Softening point of 105°C and HDT of 86°C ensure dependable performance under moderate heat exposure.

3. Easy-to-Mold Efficiency

With a 5.0 cm³/10min melt flow rate, it enables smooth, consistent injection molding for large-scale manufacturing.