Zhenjiang Chimei Kibisan® PN-108L125

zhenjiang chimei san resin as resin 25kg package

Kibisan® PN-108L125 SAN General Grade Very Light Blue

KIBISAN® PN-108L125 is a general-purpose SAN plastic resin, featuring excellent rigidity, clarity, and dimensional stability. With its very light blue hue, this material is perfect for applications demanding a blend of aesthetics and durability.

Associated Documents

ISO TDS - Data Sheet
ASTM TDS - Data Sheet
UL Product iQ
Processing Data
MSDS - Safety Data Sheet
REACH SVHC

Typical property data

Physical Properties
  • Density: 1.07 (ISO 1183, 23°C)
  • Melt Flow Rate (MFR): 5.0 cm³/10 min (ISO 1133, 200°C, 5 kg)
Mechanical Properties
  • Tensile Strength: 67 MPa (ISO 527, 50 mm/min)
  • Elongation at Break: 5.0% (ISO 527, 50 mm/min)
  • Flexural Strength: 101 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 3.4 GPa (ISO 178, 2 mm/min)
  • Hardness: M-83 (ASTM D785, M-Scale)
Impact Properties
  • IZOD Impact Strength: 3.8 kJ/m² (ISO 180, 4 mm/23°C)
Thermal Properties
  • Vicat Softening Point: 105°C (ISO 306, 50°C/hr)
  • Heat Deflection Temperature (HDT, Unannealed): 86°C (ISO 75-2)
Flame Characteristics
  • Burning Rate: 1.5 mm HB (UL File No. E194560)

Use & Applications

  • Food containers
  • Cosmetic cases
zhenjiang chimei san resin as resin 25kg package

Features & Benefits

1. Superior Mechanical Strength

It provides tensile strength of 67 MPa and outstanding rigidity, ensuring durability for high-load industrial applications.

2. Excellent Thermal Resistance

It withstands heat up to 105°C, making it reliable for products exposed to operational or environmental heat.

Smooth Mold Processing

Melt flow rate of 5.0 cm³/10 min ensures efficient molding, reducing production time and material waste.