Physical Properties
  • Density: 1.07 (ISO 1183, 23℃)
  • Melt Flow Rate (MFR): 34.0 cm³/10 min (ISO 1133, 220℃, 10 kg)
Mechanical Properties
  • Tensile Strength: 71 MPa (ISO 527, 50 mm/min)
  • Elongation at Break: 5.0% (ISO 527, 50 mm/min)
  • Flexural Strength: 106 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 3.4 GPa (ISO 178, 2 mm/min)
  • Hardness: M-83 (ASTM D785, M-Scale)
Impact Properties
  • Izod Impact Strength: 3.8 kJ/m² (ISO 180, 4 mm/23℃)
Thermal Properties
  • Vicat Softening Point: 105℃ (ISO 306, 50℃/hr)
  • Heat Deflection Temperature (HDT, Unannealed): 86℃ (ISO 75-2, Unannealed)
Flame Characteristics
  • Flammability Rating: 1.5 mm HB (UL File No.E194560, standard UL 94)

Use & Applications

  • Daily necessities
  • Cosmetic cases
  • Transparent household hardware items
zhenjiang chimei san resin as resin 25kg package

Features & Benefits

1. Crystal-Clear Transparency

KIBISAN® PN-118L100 provides excellent clarity, enhancing the aesthetics of consumer products like displays and containers.

2. High Strength and Rigidity

With outstanding tensile and flexural properties, PN-118L100 ensures durability for engineering and structural components.

3. Superior Thermal Stability

Its 105°C Vicat softening point ensures reliable performance in heat-exposed applications like appliances and electronics.