Plastic Granules
Kibisan® PN-118L150 SAN General Grade Light Blue Color
KIBISAN® PN-118L150, a general-grade SAN (Styrene Acrylonitrile) plastic, offers exceptional mechanical strength, thermal stability, and clarity in applications. With its sleek light blue appearance, it ensures consistent performance across industrial and consumer product designs.
Typical property data
Physical Properties
- Density: 1.07 g/cm³ (ISO 1183, 23°C)
- Melt Flow Rate: 34.0 cm³/10min (ISO 1133, 220°C, 10Kg)
Mechanical Properties
- Tensile Strength: 71 MPa (ISO 527, 50 mm/min)
- Elongation: 5.0% (ISO 527, 50 mm/min)
- Flexural Strength: 106 MPa (ISO 178, 2 mm/min)
- Flexural Modulus (Elasticity): 3.4 GPa (ISO 178, 2 mm/min)
- Hardness: M-83 (ASTM D785, M-Scale)
Impact Properties
- IZOD Impact Strength: 3.8 kJ/m² (ISO 180, 4 mm, 23°C)
Thermal Properties
- Vicat Softening Temperature: 105°C (ISO 306, 50°C/hour)
- Heat Distortion Temperature (HDT): 86°C (ISO 75-2, unannealed)
Flame Characteristics
- Flammability: 1.5mm HB (UL & C-UL, File No. E194560)
Use & Applications
- Daily necessities
- Cosmetic cases
Features & Benefits
1. Exceptional Mechanical Strength
With 71 MPa tensile strength, PN-118L150 ensures durable, long-lasting components for demanding industrial applications.
2. Outstanding Thermal Resistance
It can withstand up to 105°C without deformation, making it perfect for high-heat environments and precision tools.
3. Efficient Moldability
The 34 cm³/10min melt flow rate ensures fast, detailed, and cost-effective production of high-quality parts.