Zhenjiang Chimei Kibisan® PN-128L100

zhenjiang chimei san resin as resin 25kg package

Kibisan® PN-128L100 SAN General Grade Natural Color

KIBISAN® PN-128L100 is a high-performance, general-grade SAN resin, engineered for heat resistance and superior strength. In a natural color profile, it’s perfect for industries demanding reliable, durable, and versatile materials for everyday and specialized applications.

Associated Documents

ISO TDS - Data Sheet
ASTM TDS - Data Sheet
UL Product iQ
Processing Data
MSDS - Safety Data Sheet
REACH SVHC

Typical property data

Physical Properties
  • Melt Flow Rate (MFR): 34.0 cm³/10 min (ISO 1133, 220°C, 10 kg)
  • Density: 1.07 (ISO 1183, 23°C)
  • Hardness: M-84 (ASTM D785, M-Scale)
Mechanical Properties
  • Tensile Strength: 72 MPa (ISO 527, 50 mm/min)
  • Elongation at Break: 5% (ISO 527, 50 mm/min)
  • Flexural Strength: 110 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 3.6 GPa (ISO 178, 2 mm/min)
Impact Properties
  • IZOD Impact Strength: 3.9 kJ/m² (ISO 180, 4 mm/23°C)
Thermal Properties
  • Softening Point (Vicat): 107°C (ISO 306, 50°C/hr)
  • Heat Deflection Temperature (HDT): 88°C (ISO 75-2, not annealed)
Flame Characteristics
  • Flammability Rating: HB (File No. E194560, UL 94, 1.5 mm)

Use & Applications

  • Ballpoint pen casings
  • Transparent components for electrical and electronic products
  • Electric fan blades
zhenjiang chimei san resin as resin 25kg package

Features & Benefits

1. Superior Heat Resistance

Withstanding up to 88°C (HDT), PN-128L100 is perfect for high-temperature applications like appliance parts.

2. Excellent Mechanical Strength

Its 72 MPa tensile strength and 110 MPa flexural strength ensure durability in demanding industrial environments.

3. High Processability Efficiency

A melt flow rate of 34.0 cm³/min makes PN-128L100 ideal for fast, consistent, and cost-effective molding.

zhenjiang chimei san resin as resin 25kg package