Zhenjiang Chimei Kibisan® PN-128L150

zhenjiang chimei san resin as resin 25kg package

Kibisan® PN-128L150 SAN General Grade Light Blue Color

KIBISAN® PN-128L150, crafted by Zhenjiang Chimei, is a premium, heat-resistant, general-grade SAN (styrene-acrylonitrile) resin. Light blue in appearance, it boasts exceptional mechanical strength, clarity, and processability, making it perfect for diverse industrial applications.

Associated Documents

ISO TDS - Data Sheet
ASTM TDS - Data Sheet
UL Product iQ
Processing Data
MSDS - Safety Data Sheet
REACH SVHC

Typical property data

Physical Properties
  • Density: 1.071.07 g/cm³ (ISO 1183, 23°C)
  • Melt Flow Rate (MFR): 34.034.0 cm³/10 min (ISO 1133, 220220°C, 10 kg)
Mechanical Properties
  • Tensile Strength: 7272 MPa (ISO 527, 50 mm/min)
  • Elongation: 5.05.0% (ISO 527, 50 mm/min)
  • Flexural Strength: 110110 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 3.63.6 GPa (ISO 178, 2 mm/min)
Impact Properties
  • IZOD Impact Strength: 3.93.9 kJ/m² (ISO 180, 4 mm/23°C)
Thermal Properties
  • Softening Point: 107107°C (ISO 306, 50°C/hr)
  • Heat Deflection Temperature (H.D.T): 8888°C (ISO 75-2, unannealed)
Flame Characteristics
  • Burning Rate: HB rating at 1.51.5 mm thickness (File No. E194560, UL & C-UL)

Use & Applications

  • Ballpoint pen casings
  • Transparent components for electrical and electronic products
  • Electric fan blades
zhenjiang chimei san resin as resin 25kg package

Features & Benefits

1. Exceptional Heat Resistance

With a softening point of 107°C, PN-128L150 ensures durability in high-temperature industrial environments.

2. Outstanding Mechanical Strength

Delivering 72 MPa tensile strength, this resin supports creating tough, long-lasting components that endure stress.

3. Seamless Injection Molding

A high melt flow rate of 34 cm³/10 min simplifies processing, boosting production efficiency and cost savings.

zhenjiang chimei san resin as resin 25kg package