Zhenjiang Chimei Polylac® D-1000

chimei abs resin package

Polylac® D-1000 Flame Retardant Grade Standard Flow

Polylac® D-1000 is a premium flame-retardant ABS plastic resin featuring standard flow, excellent mechanical strength, and reliable thermal stability. Rated UL 94 V-0 at 1.5mm and 5VA at 3.0mm, this TBBA-based material is designed to meet rigorous safety and performance needs.

Download PDF

ISO TDS - Data Sheet
UL Product IQ
Processing Data
MSDS - Safety Data Sheet
REACH SVHC

Typical property data

Physical Properties
  • Melt Flow Rate (MFR):
    • 200°C, 5 kg: 5.5 cm³/10 min (ISO 1133)
    • 220°C, 10 kg: 58 cm³/10 min (ISO 1133)
  • Density: 1.19 g/cm³ (ISO 1183, 23°C)
  • Hardness: R-100 (ASTM D785)
Mechanical Properties
  • Melt Flow Rate (MFR):
    • 200°C, 5 kg: 5.5 cm³/10 min (ISO 1133)
    • 220°C, 10 kg: 58 cm³/10 min (ISO 1133)
  • Density: 1.19 g/cm³ (ISO 1183, 23°C)
  • Hardness: R-100 (ASTM D785)
Impact Properties
  • Tensile Strength: 37 MPa (ISO 527, 50 mm/min)
  • Flexural Strength: 63 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 2.2 GPa (ISO 178, 2 mm/min)
  • Elongation at Break: 15% (ISO 527, 50 mm/min)
Thermal Properties
  • HDT (Heat Deflection Temperature) under 1.8 MPa:
    • Annealed: 83°C (ISO 75-2)
    • Unannealed: 71°C (ISO 75-2)
  • Softening Point: 90°C (ISO 306, 10N, 50°C/hr)
Flame Characteristics
  • UL Flammability Rating:
    • 1.5 mm: V-0 (UL 94, File No. E194560)
    • 3.0 mm: 5VA (UL 94, File No. E194560)

Use & Applications

  • Set-top boxes
  • Power switch panels
  • Power sockets
  • Car batteries
  • Cash register housings
  • Light boxes
  • DVD players
  • Car audio control panels
chimei abs resin package

Features & Benefits

1. Advanced Flame-Retardant Performance

Polylac® D-1000 exceeds safety requirements with UL 94 V-0 at 1.5mm and 5VA ratings, ensuring fire protection for critical applications.

2. Outstanding Mechanical Durability

With high tensile strength (37 MPa) and excellent flexural performance (63 MPa), it’s engineered for demanding, long-lasting applications.

3. Reliable High-Heat Resistance

An HDT of 83°C (annealed) ensures dimensional stability, making it ideal for high-temperature environments in various industries.

chimei abs resin package

D-1000 Related Flame Retardant Grades

TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
Flame Retardant ABSD-1200Zhenjiang ChimeiPOLYLAC®High-rigidity FR; 2.5mm V-0 & 3.0mm V-0; Flexural 65 MPa; Hardness R-102; MFR 47; Vicat 92°CFR appliance housings; electrical enclosures; business machine covers; thick-wall rigid parts
Flame Retardant ABSD-1400Zhenjiang ChimeiPOLYLAC®High impact & elongation FR; 2.0mm V-2, 3.0mm V-0; Izod 20 kJ/m²; Elongation 25%; Vicat 94°C; GWFI 960°CFR office equipment housings; monitor & TV back covers; battery casings; appliance thick-wall parts

← Back to Chimei Flame Retardant ABS Resin — view the full POLYLAC® FR-ABS portfolio, UL 94 ratings and processing guide.

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.