Plastic Granules
Polylac® D-190 Extrusion Grade High Impact Strength
Polylac® D-190 is a high-performance general-purpose ABS plastic resin, designed for applications requiring high gloss, superior rigidity, and excellent mechanical strength. Its stable physical properties and versatile applications provide reliable solutions for industries worldwide, from electronics to consumer goods.
Typical property data
Physical Properties
- Melt Flow Rate (MFR):
- At 200°C, 5 kg: 2.1 cm³/10 min (ISO 1133)
- At 220°C, 10 kg: 22 cm³/10 min (ISO 1133)
- Density: 1.04 g/cm³ (ISO 1183)
Mechanical Properties
- Tensile Strength: 48 MPa (ISO 527, 50 mm/min)
- Elongation: 15% (ISO 527, 50 mm/min)
- Flexural Strength: 78 MPa (ISO 178, 2 mm/min)
- Flexural Modulus: 2.3 GPa (ISO 178, 2 mm/min)
- Hardness: R-105 (ASTM D785)
Impact Properties
- Izod Impact Strength (23°C): 14 kJ/m² (ISO 180, 4 mm)
- Charpy Impact Strength (23°C): 15 kJ/m² (ISO 179, 4 mm)
Thermal Properties
- Softening Temperature: 104°C (ISO 306, 10N, 50°C/hr)
- Heat Deflection Temperature (HDT):
- Annealed (1.8 MPa): 95°C (ISO 75-2)
- Unannealed (1.8 MPa): 80°C (ISO 75-2)
Flame Characteristics
- UL Rating: 1.5 mm HB (File No. E194560, UL & C-UL)
Use & Applications
- Consumer Electronics – Telephone housings
- Lighting & Household Items – lamp holders
- Toys and Crafts
- Office Essentials/office supplies
- Olock casings
- Small home appliances
Features & Benefits
1. High Gloss Surface Finish
Polylac® D-190 delivers a superior high-gloss finish, adding a professional and polished appearance to finished products.
2. Outstanding Mechanical Strength
With excellent rigidity and 78 MPa flexural strength, this resin ensures long-term structural durability under stress.
3. Reliable Thermal Stability
Designed for heat resilience, Polylac® D-190 maintains performance even in warm environments, with HDT up to 95°C.