Zhenjiang Chimei Polylac® PA-757KF

chimei abs resin package

Polylac® PA-757KF Low Residual Monomer Grade

Polylac® PA-757KF is a food-grade ABS plastic with low residual monomer content. It’s compliant with GB4806 standards, making it safe for food-contact applications. This resin delivers strength, durability, and easy processability for a wide range of industries.

Associated Documents

ISO TDS - Data Sheet
UL Product IQ
Processing Data
MSDS - Safety Data Sheet
REACH SVHC

Typical property data

Physical Properties
  • Melt Flow Rate (MFR):
    • 1.6 cm³/10 min (ISO 1133, 200℃, 5 kg)
    • 18 cm³/10 min (ISO 1133, 220℃, 10 kg)
  • Hardness: R-116 (ASTM D785)
  • Density: 1.04 g/cm³ (ISO 1183, 23℃)
Mechanical Properties
  • Tensile Strength: 46 MPa (ISO 527, 50 mm/min)
  • Elongation at Break: 20% (ISO 527, 50 mm/min)
  • Flexural Strength: 69 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 2.4 GPa (ISO 178, 2 mm/min)
Impact Properties
  • Izod Impact Strength: 18 kJ/m² (ISO 180, 4 mm, 23℃)
  • Charpy Impact Strength: 20 kJ/m² (ISO 179, 4 mm, 23℃)
Thermal Properties
  • Vicat Softening Temperature: 103℃ (ISO 306, 10N, 50℃/hr)
  • Heat Deflection Temperature (HDT):
    • 98℃ (ISO 75-2, 1.8 MPa, annealed)
    • 83℃ (ISO 75-2, 1.8 MPa, unannealed)
Flame Characteristics
  • Flammability Rating: HB at 1.5 mm thickness (UL Test, File No. E194560)

Use & Applications

  • Food containers
  • Small household appliances
chimei abs resin package

Features & Benefits

1. Food-Safe Certified Material

Polylac® PA-757KF meets GB4806 standards, ensuring safety for food-contact products like containers and kitchen tools.

2. Superior Mechanical Strength

With 46 MPa tensile strength, this resin guarantees dependable durability for automotive parts and heavy-duty consumer goods.

3. Efficient for Injection Molding

Its 18 cm³/10 min melt flow rate ensures fast, smooth molding for high-precision and high-volume manufacturing needs.

chimei abs resin package