Zhenjiang Chimei Wonderloy® PC-345KP

chimei wonderloy pc alloy pc abs resin 25kg package

Wonderloy® PC-345KP PC/ABS Eleplating Grade

Wonderloy® PC-345KP is an electroplating-grade PC/ABS alloy resin offering medium-to-high strength, excellent impact resistance, and superior thermal performance. Applications: Electroplated automotive parts, electroplated housings.

Associated Documents

ISO TDS - Data Sheet
UL Product iQ
Processing Data
MSDS - Safety Data Sheet
REACH SVHC

Typical property data

Physical Properties
  • Melt Flow Rate (MFR): 15 cm³/10min (ISO 1133, 260°C, 5kg)
  • Density: 1.10 g/cm³ (ISO 1183)
Mechanical Properties
  • Tensile Strength: 46 MPa (ISO 527, 50 mm/min)
  • Elongation: 90% (ISO 527, 50 mm/min)
  • Flexural Strength: 65 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 2.1 GPa (ISO 178, 2 mm/min)
  • Hardness: 115 HRR (ASTM D785, 1/2”)
Impact Properties
  • Izod Impact Strength (Notched): 40 kJ/m² (ISO 180, 3.2 mm/23℃)
  • Charpy Impact Strength (Notched): 42 kJ/m² (ISO 179, 3.2 mm/23℃)
Thermal Properties
  • Softening Temperature:
    • 130°C (ISO 306, 10N, 50℃/hr)
    • 112°C (ISO 306, 50N, 50℃/hr)
  • Heat Deflection Temperature (HDT):
    • 95°C at 1.8 MPa, unannealed (ISO 75-2)
    • 112°C at 0.46 MPa, unannealed (ISO 75-2)
Flame Characteristics
  • UL Flammability Rating: HB at 1.5 mm thickness (File No. E194560, UL&C-UL)

Use & Applications

  • Electroplated automotive parts
  • Electroplated housings
chimei wonderloy pc alloy pc abs resin 25kg package

Features & Benefits

1. Excellent Impact Resistance

With an Izod impact strength of 40 kJ/m² (ISO 180), Wonderloy® PC-345KP ensures durable products that withstand everyday stresses.

2. High Thermal Stability

A heat deflection temperature of 112°C (ISO 75-2) helps maintain structural integrity in demanding high-temperature environments.

3. Smooth Electroplating Performance

Specially designed for electroplating, it delivers uniform, high-quality finishes ideal for automotive and consumer electronics applications.

chimei wonderloy pc alloy pc abs resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.