Zhenjiang Chimei Wonderloy® PC-345KZ

chimei wonderloy pc alloy pc abs resin 25kg package

Wonderloy® PC-345KZ PC/ABS General Grade Medium Flow

Wonderloy® PC-345KZ PC/ABS Resin is a general-grade plastic raw material. It offers superior impact strength and heat resistance compared to ABS. Ideal for durable, heat-resistant, and stylish products in automotive, electronics, and home appliances.

Associated Documents

ISO TDS - Data Sheet
UL Product iQ
Processing Data
MSDS - Safety Data Sheet
REACH SVHC

Typical property data

Physical Properties
  • Melt Flow Index (MFI): 20 cm³/10 min (ISO 1133, 260°C, 5 kg)
  • Density: 1.1 g/cm³ (ISO 1183, 23℃)
  • Hardness: 112 HRR (ASTM D785, 1/2”)
Mechanical Properties
  • Tensile Strength: 50 MPa (ISO 527, 50 mm/min)
  • Elongation at Break: 100 % (ISO 527, 50 mm/min)
  • Flexural Strength: 75 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 2.2 GPa (ISO 178, 2 mm/min)
Impact Properties
  • Izod Impact Strength: 40 kJ/m² (ISO 180, 3.2 mm at 23℃)
  • Charpy Impact Strength: 42 kJ/m² (ISO 179, 3.2 mm at 23℃)
Thermal Properties
  • Softening Temperature:
    • 127 °C (ISO 306, 10 N, 50°C/hr)
    • 112 °C (ISO 306, 50 N, 50°C/hr)
  • Heat Deflection Temperature:
    • 95 °C (ISO 75-2, 1.8 MPa, unannealed)
    • 110 °C (ISO 75-2, 0.46 MPa, unannealed)
Flame Characteristics
  • Burning Rate: HB rating at 1.5 mm thickness (UL File No. E194560)

Use & Applications

  • Decorative Rings
  • Headlight Bases
  • Tailgate Trim Panels
chimei wonderloy pc alloy pc abs resin 25kg package

Features & Benefits

1. Superior Impact Resistance

With an impact strength of 40 kJ/m² (ISO 180), it reliably protects products from shocks and heavy usage.

2. High Heat Tolerance

Boasting a heat deflection temperature of 95°C (ISO 75-2), it excels in applications near high-temperature environments.

3. Efficient Moldability

A melt flow rate of 20 cm³/10 min (ISO 1133) ensures smooth, efficient injection molding and consistent production results.