Wonderloy® PC-365K PC/ABS Low-odor Grade Heat-resistant

Wonderloy® PC-365K is a premium PC/ABS plastic resin. It can offer low odor, low VOC emissions, and exceptional mechanical strength. Designed for demanding applications: Automotive interior components, electronic product housings, general molded parts, etc.

Associated Documents

ISO TDS - Data Sheet
UL Product iQ
Processing Data
MSDS - Safety Data Sheet
REACH SVHC

Typical property data

Physical Properties
  • Melt Flow Index (MFI): 25 cm³/10 min (ISO 1133, 260°C, 5kg)
  • Density: 1.12 g/cm³ (ISO 1183, 23°C)
  • Hardness: 115 HRR (ASTM D785, 1/2″)
Mechanical Properties
  • Tensile Strength: 55 MPa (ISO 527, 50 mm/min)
  • Elongation at Break: 120% (ISO 527, 50 mm/min)
  • Flexural Strength: 78 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 2.2 GPa (ISO 178, 2 mm/min)
Impact Properties
  • IZOD Impact Strength: 50 kJ/m² (ISO 180, 3.2 mm/23°C)
  • Charpy Impact Strength: 52 kJ/m² (ISO 179, 3.2 mm/23°C)
Thermal Properties
  • Heat Deflection Temperature (Unannealed), 1.8 MPa: 105°C (ISO 75-2)
  • Heat Deflection Temperature (Unannealed), 0.46 MPa: 125°C (ISO 75-2)
  • Vicat Softening Point, 10N: 140°C (ISO 306, 50°C/hr)
  • Vicat Softening Point, 50N: 125°C (ISO 306, 50°C/hr)
Flame Characteristics
  • UL Flammability Rating: HB at 1.5 mm thickness (File No. E194560)

Use & Applications

  • Automotive interior components
  • Electronic product housings
  • General molded parts
chimei wonderloy pc alloy pc abs resin 25kg package

Features & Benefits

1. Durable and Impact Resistant

Wonderloy® PC-365K delivers high IZOD impact strength (50 kJ/m²). Ideal for automotive panels and durable consumer products.

2. Exceptional Heat Resistance

With a softening point of up to 140°C, it withstands harsh thermal conditions. Perfect for electronics casings or under-hood automotive components.

3. Low Odor and Emissions

It ensure environmental compliance with its low VOC formulation. It is a trusted choice for interior automotive applications and eco-conscious designs.

chimei wonderloy pc alloy pc abs resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.