Wonderloy® PC-365KZ PC/ABS General Grade Heat-resistant

Wonderloy® PC-365KZ is a high-performance PC/ABS resin combining balanced mechanical strength, superior heat resistance, and excellent impact toughness, offering a reliable solution for demanding industrial applications. Perfect for Navigation systems, central console bezels, A/C air vents, advertising display frames, etc.

Associated Documents

ISO TDS - Data Sheet
UL Product iQ
Processing Data
MSDS - Safety Data Sheet
REACH SVHC

Typical property data

Physical Properties
  • Melt Flow Rate (MFR): 18 cm³/10 min (ISO 1133, 260°C, 5 kg)
  • Density: 1.13 g/cm³ (ISO 1183, 23°C)
  • Hardness: 115 HRR (ASTM D785, ½”)
Mechanical Properties
  • Tensile Strength: 55 MPa (ISO 527, 50 mm/min)
  • Elongation at Break: 120% (ISO 527, 50 mm/min)
  • Flexural Strength: 78 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 2.2 GPa (ISO 178, 2 mm/min)
Impact Properties
  • Izod Impact Strength: 45 kJ/m² (ISO 180, 3.2 mm, 23°C)
  • Charpy Impact Strength: 47 kJ/m² (ISO 179, 3.2 mm, 23°C)
Thermal Properties
  • Softening Point: 140°C (ISO 306, 10N, 50°C/hr)
    125°C (ISO 306, 50N, 50°C/hr)
  • Heat Deflection Temperature:
    • 105°C at 1.8 MPa unannealed (ISO 75-2)
    • 125°C at 0.46 MPa unannealed (ISO 75-2)
Flame Characteristics
  • Burning Rate: HB at 1.5 mm thickness (UL File No. E194560)

Use & Applications

  • Navigation systems,
  • Central console bezels
  • A/C air vents
  • Advertising display frames, etc.
chimei wonderloy pc alloy pc abs resin 25kg package

Features & Benefits

1. Superior Heat Resistance

With a heat deflection temperature of 125°C, this resin ensures durable performance under extreme thermal conditions.

2. High Impact Strength

Rated at 45 kJ/m², Wonderloy® PC-365KZ resists cracks, ensuring reliability for stress-prone components in daily use.

3. Excellent Dimensional Stability

A flexural modulus of 2.2 GPa guarantees precision, reducing warping in complex and intricately designed parts.

chimei wonderloy pc alloy pc abs resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.