Zhenjiang Chimei Wonderloy® PC-385KS

chimei wonderloy pc alloy pc abs resin 25kg package

Wonderloy® PC-385KS PC/ABS General Grade Low Temperature Resistance

Wonderloy® PC-385KS is a premium PC/ABS plastic resin. With superior impact strength, low-temperature resistance, and high heat distortion temperature, it is suitable for extrusion applications, such as Luggage and bags, safety helmets, etc.

Associated Documents

ISO TDS - Data Sheet
UL Product iQ
Processing Data
MSDS - Safety Data Sheet
REACH SVHC

Typical property data

Physical Properties
  • Melt Flow Rate: 13 cm³/10 min (ISO 1133, 260°C, 5 kg)
  • Density: 1.15 g/cm³ (ISO 1183, 23°C)
  • Hardness: 115 HRR (ASTM D785, 1/2″)
Mechanical Properties
  • Tensile Strength: 55 MPa (ISO 527, 50 mm/min)
  • Elongation: 140% (ISO 527, 50 mm/min)
  • Flexural Strength: 80 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 2.3 GPa (ISO 178, 2 mm/min)
Impact Properties
  • Izod Impact Strength: 50 kJ/m² (ISO 180, 3.2 mm, 23°C)
  • Charpy Impact Strength: 47 kJ/m² (ISO 179, 3.2 mm, 23°C)
Thermal Properties
  • Softening Point:
    • 133°C (ISO 306, 10N, 50°C/hour)
    • 143°C (ISO 306, 50N, 50°C/hour)
  • Heat Deflection Temperature:
    • 110°C at 1.8 MPa, unannealed (ISO 75-2)
    • 130°C at 0.46 MPa, unannealed (ISO 75-2)
Flame Characteristics
  • Burning Rate: HB at 1.5 mm thickness (UL File No. E194560)

Use & Applications

  • Luggage and bags
  • Safety helmets
chimei wonderloy pc alloy pc abs resin 25kg package

Features & Benefits

1. Exceptional Impact Resistance

Designed for industries requiring durability, Wonderloy® PC-385KS ensures structural integrity with an impact strength of 50 kJ/m² (ISO 180).

2. Reliable at Low Temperatures

This material excels in applications needing cold-weather resilience, keeping operations running smoothly.

3. Superior Heat Tolerance

With a heat distortion temperature of 110°C at 1.8 MPa (ISO 75-2), it withstands high-stress conditions effectively.

chimei wonderloy pc alloy pc abs resin 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.