Plastic Granules
Wonderloy® PC-6201 PC/ABS Flame-retardant Grade
Wonderloy® PC-6201 is a premium flame-retardant PC/ABS alloy. It offers superior thermal stability, excellent low-temperature impact resistance, and a UL94 V0 rating at 3.0 mm. This material is tailor-made for Miners’ safety helmets, communication products.
Typical property data
Physical Properties
- Melt Flow Rate (MFR): 6 cm³/10min (ISO 1133, 260℃, 2.16 kg)
- Density: 1.17 g/cm³ (ISO 1183, 23℃)
- Hardness: 122 HRR (ASTM D785, 1/2″)
Mechanical Properties
- Tensile Strength: 55 MPa (ISO 527, 50 mm/min)
- Elongation at Break: 110% (ISO 527, 50 mm/min)
- Flexural Strength: 70 MPa (ISO 178, 2 mm/min)
- Flexural Modulus: 2.15 GPa (ISO 178, 2 mm/min)
Impact Properties
- Izod Impact Strength: 55 kJ/m² (ISO 180, 3.2 mm, 23℃)
- Charpy Impact Strength: – (ISO 179, 3.2 mm, 23℃)
Thermal Properties
- Heat Deflection Temperature (HDT):
- 1.8 MPa unannealed: 98℃ (ISO 75-2)
- 0.46 MPa unannealed: –
- Vicat Softening Temperature:
- 10N, 50℃/hr: 123℃ (ISO 306)
- 50N, 50℃/hr: –
Flame Characteristics
- Flammability Rating: UL94 V-0 (3.0 mm, File No. E194560)
Use & Applications
- Miners’ safety helmets
- Communication products
Features & Benefits
1. Flame-Retardant with V0 Rating
Wonderloy® PC-6201 achieves a UL94 V0 rating at 3.0 mm, delivering optimal flame resistance for safety-critical applications.
2. High Heat Resistance
With a 98°C deflection temperature at 1.8 MPa, this resin withstands high-temperature environments, ensuring lasting performance.
3. Excellent Impact Strength
This material provides 55 kJ/m² Izod impact resistance, maintaining toughness for demanding applications in extreme or rough conditions.