ZPC ZA0210 ABS Resin

zpc abs granules

ZPC ZA0210 General ABS High Gloss High Stiffness

ZPC ABS ZA0210 is a high-performance ABS plastic resin offering exceptional high gloss, remarkable stiffness, and excellent processability. Perfect for manufacturing durable, aesthetically superior components in home appliances, electronics, and consumer goods.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Mass Density: 1.04 g/cm³ (GB/T 1033.1, 23 ℃)
  • Melt Flow Rate (MFR): 20 g/10 min (GB/T 3682.1, 220 ℃/10 kg)
  • Mold Shrinkage: 0.4–0.7% (GB/T 17037.4)
  • Rockwell Hardness (R-Scale): 109 (GB/T 3398.2)
Mechanical Properties
  • Tensile Strength: 44 MPa (GB/T 1040.2, 50 mm/min)
  • Flexural Strength: 68 MPa (GB/T 9341, 2 mm/min)
  • Flexural Modulus: 2.4 GPa (GB/T 9341, 2 mm/min)
  • Charpy Impact Strength (Notched, 23 ℃): 22 KJ/m² (GB/T 1043.1)
Thermal Properties
  • Heat Distortion Temperature (HDT, 1.8 MPa, unannealed): 83 ℃ (GB/T 1634.2)
  • Vicat Softening Temperature (50 N, 50 ℃/hr): 95 ℃ (GB/T 1633)
Flame Characteristics
  • Flame Rating: HB at 1.5 mm (UL-94)
Processing Parameters
  • Drying Temperature: 75–85 ℃
  • Drying Time: 2–4 hours
  • Barrel Temperature: 180–220 ℃
  • Nozzle Temperature: 200–220 ℃
  • Mold Temperature: 40–70 ℃
  • Back Pressure: 10–30 bar
  • Screw Speed: 30–60 rpm

Use & Applications

  • Home appliances
  • Electronic and electrical products
zpc abs za0210 particles

Features & Benefits

1. High Gloss and Stiffness

ZPC ABS ZA0210 is ideal for applications needing surface shine and mechanical strength.

2. Versatile Usability

Suitable for home appliances, electronics, and electrical products.

3. Efficient Processing

Excellent mold shrinkage control (0.4–0.7%) and high fluidity (MFR: 20 g/10 min).

4. Thermal Durability

With its Vicat Softening Temperature of 95 ℃ and Heat Distortion Temperature of 83 ℃, it offers reliable performance in warm environments.