SABIC® PC Resin

Sabic Polycarbonate (PC)

Sabic PC Resin, produced by SABIC’s advanced Nansha facility, is renowned for its superior optical clarity, impact resistance, and versatile engineering properties. These premium polycarbonate materials are widely used across industries such as electronics, automotive, construction, and lighting.

As a trusted supplier, we offer stable and reliable access to Sabic PC granules, meeting stringent global safety standards (RoHS, REACH) while providing exceptional performance for a wide range of applications. Choose Sabic PC resin for unparalleled strength and dependability.

polycarbonate pc resin

Sabic PC available for bulk purchase

Type Grade No. Manufacturer Brand Grade/Features Use/Applications
PC ALS01 Sabic Sabic Injection Molding Grade. Medium-low flow (MFR13), heat and UV stabilized, polycarbonate product with mold release for use in the automotive lens market.
PC ALS02 Sabic Sabic Injection Molding Grade. medium-high flow (MFR23), heat and UV stabilized, polycarbonate product with mold release for use in the automotive lens market.
PC PC0700 Sabic Sabic Compounding Grade. low flow (MFR = 7 at 300°C/1.2kg), heat stabilized for use in the custom compounding market.
PC PC0703R Sabic Sabic Extrusion grade. low flow (MFR = 7 at 300°C/1.2kg), heat and UV stabilized for use in the extrusion market
PC PC0800 Sabic Sabic Compounding Grade. low flow (MFR = 8 at 300°C/1.2kg), heat stabilized for use in the custom compounding market.
PC PC1000 Sabic Sabic Compounding Grade. medium-low flow (MFR = 10 at 300°C/1.2kg), heat stabilized, for use in the custom compounding market.
PC PC1000R Sabic Sabic Injection Molding Grade. medium-low flow (MFR = 10 at 300°C/1.2kg), heat stabilized, for use in the general purpose molding market
PC PC1003R Sabic Sabic Injection Molding Grade. medium-low flow (MFR = 10 at 300°C/1.2kg), heat and UV stabilized for use in the general purpose molding market
PC PC1004R Sabic Sabic Injection Molding Grade. Medium-low flow (MFR = 10 at 300°C/1.2kg), natural, heat stabilized, for use in the general purpose molding market
PC PC1800 Sabic Sabic Compounding Grade. Medium-low flow (MFR = 18 at 300°C/1.2kg), heat stabilized, for use in the custom compounding market.
PC PC1800R Sabic Sabic Injection Molding Grade. Medium-low flow (MFR = 18 at 300°C/1.2kg), heat stabilized, for use in the general purpose molding market
PC PC1803R Sabic Sabic Injection Molding Grade. Medium-low flow (MFR = 18 at 300°C/1.2kg),heat and UV stabilized for use in the general purpose molding market
PC PC1804R Sabic Sabic Injection Molding Grade. Medium-low flow (MFR = 18 at 300°C/1.2kg),natural, heat stabilized for use in the general purpose molding market
PC PC2200 Sabic Sabic Compounding Grade. high flow (MFR = 22 at 300°C/1.2kg), heat stabilized for use in the custom compounding market.
PC PC2200R Sabic Sabic Injection Molding Grade. High flow (MFR = 22 at 300°C/1.2kg), heat stabilized for use in the general purpose molding market
PC PC2203R Sabic Sabic Injection Molding Grade. High flow (MFR = 22 at 300°C/1.2kg), heat and UV stabilized for use in the general purpose molding market
PC PC5800 Sabic Sabic Optical Grade. very high flow (MFR = 8.9 at 250°C/1.2kg) for use in the optical media market.

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.